Nd SrTiO3 Neodymium Doped Strontium Titanate Crystal and Substrates
SKU: CS0067
To better serve you, we would like to discuss your specific requirement.
Please Contact Us for a quote.
Specifications:
Crystal Structure: Cubic
Growth Method: Vernuil Method
Lattice Parameter: a=3.905 Å
Nd Doping Concentrations: 0.05%
Melting Point: 2080°C
Density: 5.122 g/ccm
Hardness: 6-6.5 Mohs
Thermal expansion: 9.4 x 10-6/K
Dielectric Loss: ~ 5x10-4 (300k), ~ 3x10-4 (77k)
Sizes Available: 1" dia x 3mm, 1" dia x 5mm, 1" dia x 10mm, 1" dia x 15mm, 2" dia x 15mm, other sizes are available upon request
Orientations: <100>, <110>, <111>
Miscut: 0.5 degree
Polish: single or double sided
Packing: Packing in class 1000 clean room with class 100 grade plastic bag